Chemical Specifications


Mo Content(*): 99.80% min.
Al: 20 ppm max.
C: 50 ppm max.
Ca: 10 ppm max.
Co: 10 ppm max.
Cr: 10 ppm max.
Cu: 10 ppm max.
Fe: 50 ppm max.
K: 40 ppm max.
Mg: 10 ppm max.
Mn: 10 ppm max.
N: 50 ppm max.
Na: 20 ppm max.
Ni: 10 ppm max.
O: 200 ppm max.
Pb: 20 ppm max.
S: 10 ppm máx.
Si: 35 ppm máx.
W: 300 ppm max.

(*)Excluding gas content.

Physical Properties


Typical size 60 x 40 x 20 mm approx.
Shape irregular 2,35x1,75x0,78 pulgadas approx.

Further elements and specifications upon request.

Packaging Options


Packing unit Content per unit
Steel drums, polyethylene lined 100 – 250 kg Mo
<
Other packaging upon request.


Handling instructions


When handling the material the working instructions valid in each country must be adhered to.


Camino Nos a Los Morros N° 66, San Bernardo, Chile  +(56-2) 937 6600 +(56-2) 937 6600  +(56-2) 937 6653 +(56-2) 937 6653  info@molymet.cl info@molymet.cl